AISI CW-5

Location » Home » Grades > Special Alloy > CW-5

Grades | Special Alloy | CW-5

AISI CW-5

Print

CW-5 Application:W-Ta-Nb-Ti-Co class carbide

Chemical composition(mass fraction)(wt.%) of the CW-5
C(%) W(%) Co(%) Nb(%) Ti(%) Ta(%)
6.2 75.3 8.5 1.6 3.2 5.2

Mechanical properties of grade CW-5

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
181 (≥) 167 (≥) 43 13 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade CW-5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
236 (≥) 153 (≥) 31 43 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
288 215 567 - - -

CW-5 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED