AISI ASTM LCC

Location » Home » Grades > Special Alloy > ASTM LCC

Grades | Special Alloy | ASTM LCC

AISI ASTM LCC

Print

Chemical composition(mass fraction)(wt.%) of the ASTM LCC
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) Cu(%)
Max 0.25 Max 0.60 Max 1.20 Max 0.040 Max 0.045 Max 0.50 Max 0.50 Max 0.20 Max 0.03 Max 0.30

Mechanical properties of grade ASTM LCC

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
468 (≥) 254 (≥) 44 34 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade ASTM LCC

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
776 (≥) 283 (≥) 34 23 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
765 339 646 - - -

ASTM LCC Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED