AISI UNS J91540

Location » Home » Grades > Special Alloy > UNS J91540

Grades | Special Alloy | UNS J91540

AISI UNS J91540

Print

Chemical composition(mass fraction)(wt.%) of the UNS J91540
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%)
Max 0.06 Max 1.00 Max 1.00 Max 0.040 Max 0.03 11.5-14.0 3.50-4.50 0.40-1.00

Mechanical properties of grade UNS J91540

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
975 (≥) 732 (≥) 32 33 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade UNS J91540

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
172 (≥) 167 (≥) 21 44 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
136 415 271 - - -

UNS J91540 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED