Chemical composition(mass fraction)(wt.%) of the ICI 4140
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) W(%) Cu(%)
0.35-0.45 0.20-0.80 0.70-1.00 Max 0.04 Max 0.045 0.80-1.10 Max 0.50 0.15-0.25 Max 0.10 Max 0.50

Mechanical properties of grade ICI 4140

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
814 (≥) 189 (≥) 21 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade ICI 4140

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
743 (≥) 959 (≥) 23 44 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
867 761 462 - - -

ICI 4140 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED