ISO ISO 11

Location » Home » Grades > Special Alloy > ISO 11

Grades | Special Alloy | ISO 11

ISO ISO 11

Print

ISO 11 Application:ISO standard thermal deformation of stainless steel

Chemical composition(mass fraction)(wt.%) of the ISO 11
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) N(%)
Max 0.070 Max 1.00 Max 2.00 Max 0.045 Max 0.030 17.0-19.5 8.00-10.5 Max 0.11

Mechanical properties of grade ISO 11

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
472 (≥) 286 (≥) 43 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade ISO 11

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
142 (≥) 925 (≥) 22 34 13 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
237 644 192 - - -

ISO 11 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED