ISO ISO X6CrMoNb17-1

Print

ISO X6CrMoNb17-1 Application:ISO standard thermal deformation of stainless steel

Chemical composition(mass fraction)(wt.%) of the ISO X6CrMoNb17-1
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) N(%) Other(%)
Max 0.080 Max 1.00 Max 1.00 Max 0.040 Max 0.015 16.0-18.0 0.80-1.40 Max 0.040 5xC%≤Ti≤1.00

Mechanical properties of grade ISO X6CrMoNb17-1

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
663 (≥) 197 (≥) 42 41 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade ISO X6CrMoNb17-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
662 (≥) 249 (≥) 23 41 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
452 116 936 - - -

ISO X6CrMoNb17-1 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED