ISO ISO X6CrNiTi18-10 Tube

Location » Home » Grades > Special Alloy > ISO X6CrNiTi18-10 Tube

Grades | Special Alloy | ISO X6CrNiTi18-10 Tube

ISO ISO X6CrNiTi18-10 Tube

Print

ISO X6CrNiTi18-10 Tube Application:ISO standard austenitic stainless steel pressure seamless steel tube

Chemical composition(mass fraction)(wt.%) of the ISO X6CrNiTi18-10 Tube
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%)
Max 0.08 Max 1.00 Max 2.00 Max 0.040 Max 0.030 17.0-19.0 9.00-12.0

Mechanical properties of grade ISO X6CrNiTi18-10 Tube

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
981 (≥) 347 (≥) 24 32 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade ISO X6CrNiTi18-10 Tube

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
882 (≥) 216 (≥) 23 34 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
447 561 397 - - -

ISO X6CrNiTi18-10 Tube Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED