ISO X15CrN26 Application:ISO standard iron grain size heat resistant steel

Chemical composition(mass fraction)(wt.%) of the ISO X15CrN26
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) N(%)
Max 0.20 Max 1.0 Max 1.00 Max 0.040 Max 0.030 24.0-28.0 Max 1.0 0.15-0.25

Mechanical properties of grade ISO X15CrN26

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
742 (≥) 233 (≥) 42 32 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade ISO X15CrN26

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
797 (≥) 361 (≥) 42 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
916 578 575 - - -

ISO X15CrN26 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED