ISO X15CrNiSi20 12 Application:ISO standard Austenite size heat resistant steel

Chemical composition(mass fraction)(wt.%) of the ISO X15CrNiSi20 12
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Nb(%)
Max 0.10 1.5-2.5 Max 1.00 Max 0.045 Max 0.030 17.0-19.0 9.0-12.0 10x%C≤1.2

Mechanical properties of grade ISO X15CrNiSi20 12

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
866 (≥) 876 (≥) 32 23 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade ISO X15CrNiSi20 12

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
343 (≥) 546 (≥) 12 22 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
198 916 686 - - -

ISO X15CrNiSi20 12 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED