ISO X12CrNiMoV12 3 Application:High temperature bainite and martensite steel ISO standard internal combustion engine

Chemical composition(mass fraction)(wt.%) of the ISO X12CrNiMoV12 3
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) N(%) B(%)
0.08-0.15 Max 0.35 0.50-0.90 Max 0.03 Max 0.025 11.0-12.5 1.00-2.00 1.50-2.00 0.25-0.40 0.02-0.04 Max 0.008

Mechanical properties of grade ISO X12CrNiMoV12 3

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
789 (≥) 554 (≥) 23 44 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade ISO X12CrNiMoV12 3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
983 (≥) 632 (≥) 43 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
387 225 792 - - -

ISO X12CrNiMoV12 3 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED