CNS CNS 403

Location » Home » Grades > Special Alloy > CNS 403

Grades | Special Alloy | CNS 403

CNS CNS 403

Print

CNS 403 Application:CNS standard martensite stainless steel

Chemical composition(mass fraction)(wt.%) of the CNS 403
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%)
Max 0.15 Max 0.50 Max 1.00 Max 0.040 Max 0.030 11.50-13.00 Max 0.60

Mechanical properties of grade CNS 403

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
916 (≥) 294 (≥) 22 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade CNS 403

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
853 (≥) 283 (≥) 24 13 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
132 878 283 - - -

CNS 403 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED