KS STS420J1TKA

Location » Home » Grades > Special Alloy > STS420J1TKA

Grades | Special Alloy | STS420J1TKA

KS STS420J1TKA

Print

STS420J1TKA Application:KS standard mechanical and structure with stainless steel pipe(KS D3536-1992)

Chemical composition(mass fraction)(wt.%) of the STS420J1TKA
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%)
0.16-0.25 Max 1.00 Max 1.00 Max 0.04 Max 0.03 12.0-14.0 Max 0.60

Mechanical properties of grade STS420J1TKA

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
365 (≥) 916 (≥) 14 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade STS420J1TKA

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
925 (≥) 455 (≥) 41 31 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
346 988 564 - - -

STS420J1TKA Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED