Stellite 228

Location » Home » Grades > Special Alloy > Stellite 228

Grades | Special Alloy | Stellite 228

Stellite 228

Print

Stellite 228 Application:Stellite alloy

Chemical composition(mass fraction)(wt.%) of the Stellite 228
C(%) Cr(%) Mo(%) Co(%) Other(%)
0.1 26.0 3.0 remaining Fe:20.0

Mechanical properties of grade Stellite 228

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
513 (≥) 956 (≥) 21 22 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade Stellite 228

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
232 (≥) 823 (≥) 22 44 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
561 445 921 - - -

Stellite 228 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED