SS SS 2662

Location » Home » Grades > Special Alloy > SS 2662

Grades | Special Alloy | SS 2662

SS SS 2662

Print

SS 2662 Application:Swedish SS standard stainless steel and heat resistant steel

Chemical composition(mass fraction)(wt.%) of the SS 2662
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Cu(%)
Max 0.025 Max 1.0 Max 2.0 Max 0.03 Max 0.02 19.0-21.0 24.0-26.0 4.0-5.0 1.2-2.0

Mechanical properties of grade SS 2662

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
644 (≥) 848 (≥) 33 12 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade SS 2662

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
232 (≥) 472 (≥) 41 33 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
385 888 371 - - -

SS 2662 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED