GBT 12Cr17Mn6Ni5N

Location » Home » Grades > Special Alloy > 12Cr17Mn6Ni5N

Grades | Special Alloy | 12Cr17Mn6Ni5N

GBT 12Cr17Mn6Ni5N

Print

12Cr17Mn6Ni5N Application: Stainless steel bars

Chemical composition(mass fraction)(wt.%) of the 12Cr17Mn6Ni5N
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) N(%)
Max 0.15 Max 1.0 5.5-7.5 Max 0.05 Max 0.03 16.0-18.0 3.5-5.5 0.05-0.25

Mechanical properties of grade 12Cr17Mn6Ni5N

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
516 (≥) 597 (≥) 13 43 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 112

Physical properties of grade 12Cr17Mn6Ni5N

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
154 (≥) 174 (≥) 21 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
283 923 733 - - -

12Cr17Mn6Ni5N Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED