GBT 53Cr21Mn9Ni4N

Location » Home » Grades > Special Alloy > 53Cr21Mn9Ni4N

Grades | Special Alloy | 53Cr21Mn9Ni4N

GBT 53Cr21Mn9Ni4N

Print

53Cr21Mn9Ni4N Application:Stainless steel bars

Chemical composition(mass fraction)(wt.%) of the 53Cr21Mn9Ni4N
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) N(%)
0.48-0.58 0.35 8.0-10.0 0.04 0.03 20.0-22.0 3.25-4.5 0.35-0.5

Mechanical properties of grade 53Cr21Mn9Ni4N

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
511 (≥) 194 (≥) 44 32 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade 53Cr21Mn9Ni4N

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
888 (≥) 643 (≥) 34 24 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
467 829 687 - - -

53Cr21Mn9Ni4N Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED