22Cr20Mn10Ni2Si2N Application:Stainless steel bars

Chemical composition(mass fraction)(wt.%) of the 22Cr20Mn10Ni2Si2N
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) N(%)
0.17-0.26 1.8-2.7 8.5-11.0 0.05 0.03 18.0-21.0 2.0-3.0 0.2-0.3

Mechanical properties of grade 22Cr20Mn10Ni2Si2N

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
633 (≥) 793 (≥) 11 24 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade 22Cr20Mn10Ni2Si2N

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
916 (≥) 142 (≥) 42 11 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
732 871 655 - - -

22Cr20Mn10Ni2Si2N Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED