GBT 07Cr19Ni11Ti

Location » Home » Grades > Special Alloy > 07Cr19Ni11Ti

Grades | Special Alloy | 07Cr19Ni11Ti

GBT 07Cr19Ni11Ti

Print

07Cr19Ni11Ti Application:Stainless steel bars

Chemical composition(mass fraction)(wt.%) of the 07Cr19Ni11Ti
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Ti(%)
0.04-0.1 0.75 2.0 0.03 0.03 17.0-20.0 9.0-13.0 0.66(4C)

Mechanical properties of grade 07Cr19Ni11Ti

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
918 (≥) 232 (≥) 14 24 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade 07Cr19Ni11Ti

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
413 (≥) 774 (≥) 22 42 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
947 246 411 - - -

07Cr19Ni11Ti Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED