GBT S32652

Location » Home » Grades > Special Alloy > S32652

Grades | Special Alloy | S32652

GBT S32652

Print

S32652 Application:Stainless steel bars

Chemical composition(mass fraction)(wt.%) of the S32652
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) N(%) Cu(%) Ti(%)
0.02 0.5 2.0-4.0 0.03 0.0050 24.0-25.0 21.0-23.0 7.0-8.0 0.45-0.55 0.3-0.6 0.66(4C)

Mechanical properties of grade S32652

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
947 (≥) 981 (≥) 14 31 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade S32652

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
816 (≥) 261 (≥) 43 34 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
924 835 769 - - -

S32652 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED