Y0Cr16Ni10Ca Application:Stainless steel bars

Chemical composition(mass fraction)(wt.%) of the Y0Cr16Ni10Ca
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Cu(%) Other(%)
0.08 0.8 1.5 0.035 0.04-0.1 15.5-17.5 8.5-10.5 1.0 0.1-0.25 Ca 0.01

Mechanical properties of grade Y0Cr16Ni10Ca

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
185 (≥) 151 (≥) 22 42 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade Y0Cr16Ni10Ca

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
647 (≥) 791 (≥) 32 24 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
336 164 292 - - -

Y0Cr16Ni10Ca Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting