GBT 05Cr19Ni10Si2NbN

Location » Home » Grades > Special Alloy > 05Cr19Ni10Si2NbN

Grades | Special Alloy | 05Cr19Ni10Si2NbN

GBT 05Cr19Ni10Si2NbN

Print

05Cr19Ni10Si2NbN Application:Stainless steel bars

Chemical composition(mass fraction)(wt.%) of the 05Cr19Ni10Si2NbN
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) N(%) Other(%)
0.04-0.06 1.0-2.0 2.0 0.045 0.03 18.0-19.0 9.0-10.0 0.12-0.18 Ce 0.03-0.08

Mechanical properties of grade 05Cr19Ni10Si2NbN

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
915 (≥) 599 (≥) 32 13 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade 05Cr19Ni10Si2NbN

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
662 (≥) 498 (≥) 24 21 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
318 958 244 - - -

05Cr19Ni10Si2NbN Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED