STAS/SR 2NbNiCr250

Location » Home » Grades > Special Alloy > 2NbNiCr250

Grades | Special Alloy | 2NbNiCr250

STAS/SR 2NbNiCr250

Print

2NbNiCr250 Application:Stainless steel

Chemical composition(mass fraction)(wt.%) of the 2NbNiCr250
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Cu(%) Other(%)
≤0.03 0. 40 1.00 0.035 0.025 23.0-26.0 19.0-22,0 ≤0. 20 0.30 Nb 0.20-0. 30

Mechanical properties of grade 2NbNiCr250

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
535 (≥) 639 (≥) 31 24 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade 2NbNiCr250

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
555 (≥) 338 (≥) 21 22 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
164 992 215 - - -

2NbNiCr250 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED