STAS/SR 10AlCr70

Location » Home » Grades > Special Alloy > 10AlCr70

Grades | Special Alloy | 10AlCr70

STAS/SR 10AlCr70

Print

10AlCr70 Application:Stainless steel

Chemical composition(mass fraction)(wt.%) of the 10AlCr70
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Cu(%) Al(%)
≤0.12 0. 50-1. 00 1.00 0. 04 0.030 6.00-8.00 ≤0. 50 0. 20 0. 30 0. 50-1. 00

Mechanical properties of grade 10AlCr70

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
722 (≥) 513 (≥) 11 42 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade 10AlCr70

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
789 (≥) 553 (≥) 11 44 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
926 744 578 - - -

10AlCr70 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED