STAS/SR OLT35

Location » Home » Grades > Special Alloy > OLT35

Grades | Special Alloy | OLT35

STAS/SR OLT35

Print

OLT35 Application:Structural steel

Chemical composition(mass fraction)(wt.%) of the OLT35
C(%) Si(%) Mn(%) P(%) S(%)
0.09-0.16 0.17-0.37 0.40-0.80 0.040 0.045

Mechanical properties of grade OLT35

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
284 (≥) 952 (≥) 12 32 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade OLT35

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
577 (≥) 783 (≥) 41 31 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
899 856 248 - - -

OLT35 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED