STAS/SR 40VMoMnCr7

Location » Home » Grades > Special Alloy > 40VMoMnCr7

Grades | Special Alloy | 40VMoMnCr7

STAS/SR 40VMoMnCr7

Print

40VMoMnCr7 Application:Structural steel

Chemical composition(mass fraction)(wt.%) of the 40VMoMnCr7
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) Cu(%)
0.36-0.44 0.17-0.37 0.90-1.20 0.035 0.035 0.55-0.95 0.30 0.25-0.70 0.15-0.25 0.30

Mechanical properties of grade 40VMoMnCr7

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
449 (≥) 275 (≥) 12 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade 40VMoMnCr7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
567 (≥) 398 (≥) 44 33 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
862 551 582 - - -

40VMoMnCr7 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED