STAS/SR OI.T45K

Location » Home » Grades > Special Alloy > OI.T45K

Grades | Special Alloy | OI.T45K

STAS/SR OI.T45K

Print

OI.T45K Application:Structural steel

Chemical composition(mass fraction)(wt.%) of the OI.T45K
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Cu(%)
Max 0.23 0.15-0.35 ≥0.40 0.040 0.045 0.30 0.30 0.30

Mechanical properties of grade OI.T45K

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
942 (≥) 193 (≥) 21 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade OI.T45K

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
852 (≥) 133 (≥) 22 43 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
989 396 861 - - -

OI.T45K Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED