STAS/SR RCB52q

Location » Home » Grades > Special Alloy > RCB52q

Grades | Special Alloy | RCB52q

STAS/SR RCB52q

Print

RCB52q Application:Structural steel

Chemical composition(mass fraction)(wt.%) of the RCB52q
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) V(%) Al(%)
Max 0.18 Max 0.60 Max 1.15 0.040 0.040 0.50-0.80 Max 0.12 2*0.025 0.30-0.60

Mechanical properties of grade RCB52q

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
412 (≥) 366 (≥) 23 11 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade RCB52q

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
465 (≥) 842 (≥) 23 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
582 114 318 - - -

RCB52q Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED