STAS/SR OLC2Sq

Location » Home » Grades > Special Alloy > OLC2Sq

Grades | Special Alloy | OLC2Sq

STAS/SR OLC2Sq

Print

OLC2Sq Application:Alloy structural steel

Chemical composition(mass fraction)(wt.%) of the OLC2Sq
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Cu(%)
0.22-0.29 0.17-0.37 0.40-0.70 0.035 0.035 Max 0.30 0.3 0.3

Mechanical properties of grade OLC2Sq

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
864 (≥) 524 (≥) 21 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade OLC2Sq

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
891 (≥) 611 (≥) 31 41 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
572 879 835 - - -

OLC2Sq Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED