STAS/SR 40BCr10AT

Location » Home » Grades > Special Alloy > 40BCr10AT

Grades | Special Alloy | 40BCr10AT

STAS/SR 40BCr10AT

Print

40BCr10AT Application:Alloy structural steel

Chemical composition(mass fraction)(wt.%) of the 40BCr10AT
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Cu(%)
0.36-0.44 0.17-0.37 0.50-0.80 0.025 0.025 0.80-1.10 0.30 0.3

Mechanical properties of grade 40BCr10AT

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
621 (≥) 419 (≥) 42 21 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade 40BCr10AT

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
567 (≥) 741 (≥) 41 11 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
544 466 332 - - -

40BCr10AT Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting