STAS/SR 30VCrW85

Location » Home » Grades > Special Alloy > 30VCrW85

Grades | Special Alloy | 30VCrW85

STAS/SR 30VCrW85

Print

30VCrW85 Application:tool steel

Chemical composition(mass fraction)(wt.%) of the 30VCrW85
C(%) Si(%) Mn(%) P(%) S(%) Ni(%) Mo(%) V(%) W(%) Co(%)
0.25-0.35 0.15 -0.35 0.20-0.40 0.030 0.030 0.30- 0.40 0.35 8.00-9.00 0.3 2. 50-2.80

Mechanical properties of grade 30VCrW85

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
345 (≥) 932 (≥) 12 41 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade 30VCrW85

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
488 (≥) 969 (≥) 43 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
769 752 576 - - -

30VCrW85 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED