STAS/SR Rpl

Location » Home » Grades > Special Alloy > Rpl

Grades | Special Alloy | Rpl

STAS/SR Rpl

Print

Rpl Application:tool steel

Chemical composition(mass fraction)(wt.%) of the Rpl
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) Co(%)
0.90-1.00 Max 0.50 Max 0.50 0.030 0.030 3.80- 4.40 2.30- 2.70 Max 1.00 9.00-10,0 5.00- 6,00

Mechanical properties of grade Rpl

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
341 (≥) 269 (≥) 14 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade Rpl

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
594 (≥) 861 (≥) 24 32 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
191 315 986 - - -

Rpl Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED