STAS/SR T12TiMoNiCrl75

Location » Home » Grades > Special Alloy > T12TiMoNiCrl75

Grades | Special Alloy | T12TiMoNiCrl75

STAS/SR T12TiMoNiCrl75

Print

T12TiMoNiCrl75 Application:Cast Steel

Chemical composition(mass fraction)(wt.%) of the T12TiMoNiCrl75
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Other(%)
0.12 ≤1.00 1.00-2.00 0.035 0.030 16.0-19.0 11.0-13.0 3.00-4.00 Ti-5XC

Mechanical properties of grade T12TiMoNiCrl75

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
379 (≥) 998 (≥) 14 44 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade T12TiMoNiCrl75

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
135 (≥) 528 (≥) 42 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
638 868 491 - - -

T12TiMoNiCrl75 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED