STAS/SR T15MoNiCrl80

Location » Home » Grades > Special Alloy > T15MoNiCrl80

Grades | Special Alloy | T15MoNiCrl80

STAS/SR T15MoNiCrl80

Print

T15MoNiCrl80 Application:Cast Steel

Chemical composition(mass fraction)(wt.%) of the T15MoNiCrl80
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%)
0.15 0.50-2.00 2.00 0.040 0.030 17.0-20.0 9.00-12.0 2.00-3.00

Mechanical properties of grade T15MoNiCrl80

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
373 (≥) 831 (≥) 14 13 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade T15MoNiCrl80

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
484 (≥) 325 (≥) 24 13 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
342 651 829 - - -

T15MoNiCrl80 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED