STAS/SR T15NiCr135

Location » Home » Grades > Special Alloy > T15NiCr135

Grades | Special Alloy | T15NiCr135

STAS/SR T15NiCr135

Print

T15NiCr135 Application:Cast Steel

Chemical composition(mass fraction)(wt.%) of the T15NiCr135
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%)
0.1? ≤0.60 0.40-0.90 0.035 0.03 12.0-15.0 0.70-1.20

Mechanical properties of grade T15NiCr135

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
455 (≥) 561 (≥) 41 41 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade T15NiCr135

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
645 (≥) 665 (≥) 33 43 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
335 331 968 - - -

T15NiCr135 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED