UNE 46CrS2

Location » Home » Grades > Special Alloy > 46CrS2

Grades | Special Alloy | 46CrS2

UNE 46CrS2

Print

46CrS2 Application:Spain structural alloy steel

Chemical composition(mass fraction)(wt.%) of the 46CrS2
C(%) Si(%) Mn(%) P(%) S(%) Cr(%)
0.42-0.50 0.4 0.50-0.80 0.035 0.020-0.040 0.40-0.60

Mechanical properties of grade 46CrS2

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
414 (≥) 329 (≥) 24 21 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade 46CrS2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
751 (≥) 145 (≥) 41 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
691 737 674 - - -

46CrS2 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED