UNE X1NiCrMoCu25-20-5

Location » Home » Grades > Special Alloy > X1NiCrMoCu25-20-5

Grades | Special Alloy | X1NiCrMoCu25-20-5

UNE X1NiCrMoCu25-20-5

Print

X1NiCrMoCu25-20-5 Application:Spain structural alloy steel

Chemical composition(mass fraction)(wt.%) of the X1NiCrMoCu25-20-5
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) N(%) Cu(%)
0.020 0.70 2.00 0.030 0.010 19.0-21.0 24.0-26.0 4.00-5.00 Max 0.15 1.20-2.00

Mechanical properties of grade X1NiCrMoCu25-20-5

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
545 (≥) 998 (≥) 33 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade X1NiCrMoCu25-20-5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
225 (≥) 988 (≥) 24 41 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
326 732 384 - - -

X1NiCrMoCu25-20-5 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED