UNE X2CrNi18-9

Location » Home » Grades > Special Alloy > X2CrNi18-9

Grades | Special Alloy | X2CrNi18-9

UNE X2CrNi18-9

Print

X2CrNi18-9 Application:Spain structural alloy steel

Chemical composition(mass fraction)(wt.%) of the X2CrNi18-9
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) N(%)
0.030 1.00 2.00 0.045 0.015 17.5-19.5 8.00-10.0 Max 0.11

Mechanical properties of grade X2CrNi18-9

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
613 (≥) 679 (≥) 32 31 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade X2CrNi18-9

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
882 (≥) 449 (≥) 13 43 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
623 312 125 - - -

X2CrNi18-9 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED