UNE GX2CrNiMoN25-6-3

Location » Home » Grades > Special Alloy > GX2CrNiMoN25-6-3

Grades | Special Alloy | GX2CrNiMoN25-6-3

UNE GX2CrNiMoN25-6-3

Print

GX2CrNiMoN25-6-3 Application:Spain structural alloy steel

Chemical composition(mass fraction)(wt.%) of the GX2CrNiMoN25-6-3
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) N(%)
0.030 1.00 2.00 0.035 0.025 24.5-26.5 5.50-7.00 2.50-3.50 0.12-0.25

Mechanical properties of grade GX2CrNiMoN25-6-3

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
342 (≥) 699 (≥) 33 43 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade GX2CrNiMoN25-6-3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
824 (≥) 816 (≥) 22 33 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
891 974 296 - - -

GX2CrNiMoN25-6-3 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED