UNE GX4NiCtCuMo30-20-4

Location » Home » Grades > Special Alloy > GX4NiCtCuMo30-20-4

Grades | Special Alloy | GX4NiCtCuMo30-20-4

UNE GX4NiCtCuMo30-20-4

Print

GX4NiCtCuMo30-20-4 Application:Spain structural alloy steel

Chemical composition(mass fraction)(wt.%) of the GX4NiCtCuMo30-20-4
C(%) Si(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Cu(%)
0.06 1.50 0.040 0.030 19.0-22.0 27.5-30.5 2.00-3.00 3.00-4.00

Mechanical properties of grade GX4NiCtCuMo30-20-4

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
876 (≥) 488 (≥) 21 21 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade GX4NiCtCuMo30-20-4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
173 (≥) 437 (≥) 31 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
452 555 895 - - -

GX4NiCtCuMo30-20-4 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED