30CrMoV12 Application:Spain structural alloy steel

Chemical composition(mass fraction)(wt.%) of the 30CrMoV12
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) V(%)
0.25-0.35 0.10-0.40 0.15-0.45 0.025 0.020 2.50-3.50 2.50-3.50 0.40-0.70

Mechanical properties of grade 30CrMoV12

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
538 (≥) 937 (≥) 31 11 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade 30CrMoV12

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
935 (≥) 512 (≥) 22 22 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
829 859 446 - - -

30CrMoV12 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting