UNE HS10.4-3-10

Print

HS10.4-3-10 Application:Spain structural alloy steel

Chemical composition(mass fraction)(wt.%) of the HS10.4-3-10
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) V(%) W(%) Co(%)
1.20-1.35 Max 0.45 Max 0.40 0.030 0.025 3.50-4.50 3.20-3.90 3.00-3.50 9.00-10.0 9.50-10.5

Mechanical properties of grade HS10.4-3-10

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
962 (≥) 267 (≥) 21 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade HS10.4-3-10

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
533 (≥) 983 (≥) 34 11 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
871 339 589 - - -

HS10.4-3-10 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED