UNE 12Ni14

Location » Home » Grades > Special Alloy > 12Ni14

Grades | Special Alloy | 12Ni14

UNE 12Ni14

Print

12Ni14 Application:Spain structural alloy steel

Chemical composition(mass fraction)(wt.%) of the 12Ni14
C(%) Si(%) Mn(%) P(%) S(%) Ni(%) V(%)
0.15 0. 35 0.30—0.80 0.020 0. 010 3.25—3.75 <0.05

Mechanical properties of grade 12Ni14

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
536 (≥) 437 (≥) 12 44 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade 12Ni14

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
851 (≥) 965 (≥) 43 43 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
946 733 963 - - -

12Ni14 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED