UNE E8332

Location » Home » Grades > Special Alloy > E8332

Grades | Special Alloy | E8332

UNE E8332

Print

E8332 Application:Spain structural alloy steel

Chemical composition(mass fraction)(wt.%) of the E8332
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%)
0.38-0.45 0. 30—0. 50 0.50—0.80 0.040 0.040 0. 80—1.20 0.15-0.30

Mechanical properties of grade E8332

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
658 (≥) 253 (≥) 12 41 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade E8332

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
584 (≥) 565 (≥) 12 44 13 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
151 816 277 - - -

E8332 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED