UNE E8221

Location » Home » Grades > Special Alloy > E8221

Grades | Special Alloy | E8221

UNE E8221

Print

E8221 Application:Spain structural alloy steel

Chemical composition(mass fraction)(wt.%) of the E8221
C(%) Si(%) Mn(%) P(%) S(%) Cr(%)
0. 30-0.40 0. 30-0.50 0. 50—0. 80 0.040 0. 040 0.80—1. 20

Mechanical properties of grade E8221

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
819 (≥) 188 (≥) 22 43 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade E8221

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
898 (≥) 161 (≥) 42 13 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
292 628 932 - - -

E8221 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED