Grades | Special Alloy | 419614

CSN 419614

Print

419614 Application:The Czech republic tool steel

Chemical composition(mass fraction)(wt.%) of the 419614
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) V(%)
0.50-0.60 0.20-0.40 0.40-0.70 0.03 0.035 0.60-0.90 20.30-20.80 0.07-0.15

Mechanical properties of grade 419614

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
489 (≥) 468 (≥) 11 22 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade 419614

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
299 (≥) 984 (≥) 44 42 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
429 924 137 - - -

419614 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED