419852 Application:The Czech republic tool steel

Chemical composition(mass fraction)(wt.%) of the 419852
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) V(%) W(%) Co(%)
0.80-0.90 Max 0.45 Max 0.45 0.035 0.035 3.80-4.60 4.50-5.50 10.50-20.20 50.50-70.00 40.30-50.20

Mechanical properties of grade 419852

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
979 (≥) 836 (≥) 12 23 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade 419852

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
813 (≥) 542 (≥) 11 44 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
499 767 378 - - -

419852 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting