Grades | Special Alloy | 17 335

CSN 17 335

Print

17 335 Application:The Czech republic Stainless steel

Chemical composition(mass fraction)(wt.%) of the 17 335
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Ti(%)
0.12 0.80 1.00-2.00 0.045 0.030 13.5-16.5 34.0-38.0 1.20-1.90

Mechanical properties of grade 17 335

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
978 (≥) 459 (≥) 14 41 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade 17 335

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
421 (≥) 743 (≥) 14 44 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
986 542 731 - - -

17 335 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED