ONORM Stl3F

Location » Home » Grades > Special Alloy > Stl3F

Grades | Special Alloy | Stl3F

ONORM Stl3F

Print

Stl3F Application:Austrian structural steel

Chemical composition(mass fraction)(wt.%) of the Stl3F
C(%) Si(%) Mn(%) P(%) S(%)
0.1 0.15 0.20-0.45 0.030 0.03

Mechanical properties of grade Stl3F

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
477 (≥) 746 (≥) 13 21 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade Stl3F

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
141 (≥) 262 (≥) 12 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
243 685 669 - - -

Stl3F Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED