ONORM St35KW

Location » Home » Grades > Special Alloy > St35KW

Grades | Special Alloy | St35KW

ONORM St35KW

Print

St35KW Application:Austrian structural steel

Chemical composition(mass fraction)(wt.%) of the St35KW
C(%) Si(%) Mn(%) P(%) S(%) Al(%)
Max 0.16 Max 0.35 0.40.1.20 0.035 0.030 0.02

Mechanical properties of grade St35KW

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
315 (≥) 454 (≥) 12 34 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade St35KW

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
766 (≥) 194 (≥) 41 12 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
453 354 618 - - -

St35KW Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED