GBT 12CrlMoVg

Print

12CrlMoVg Application:China structural steel and alloy steel

Chemical composition(mass fraction)(wt.%) of the 12CrlMoVg
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) V(%)
0.08-0.15 0.17-0.37 0.40-0.70 0.03 0.03 0.90-1.20 0.25-0.35 0.15-0.30

Mechanical properties of grade 12CrlMoVg

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
894 (≥) 598 (≥) 32 24 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade 12CrlMoVg

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
524 (≥) 696 (≥) 34 41 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
168 456 164 - - -

12CrlMoVg Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED